Exaton 385-16
385-16 is a covered electrode with type with rutile-basic coating and normal recovery, used for welding of high-alloy austenitic stainless of UNS N08904 type, also known as 904L. 385-16 gives a fully austenitic chromium-nickel-molybdenum weld metal with especially low carbon content and copper addition. Spray transfer gives a bead with a finely rippled surface, little spatter and good slag removal. It is suitable for joining steels of the 20Cr/25Ni/4.5Mo/1.5Cu type such as 2RK65 and 904L used in many areas of the process industry, such as in the production of acetic acid, sulphuric acid, terephthalic or tartaric acid and vinyl chloride as well as other chloride containing media. It is also suitable for use in cooling operations involving sea water or heavily polluted river water. 385-16 may also be used to join 317L where improved corrosion resistance in specific media is required. These electrodes may be used to join 2RK65, 904L, and 317L to other grades of stainless steel.
Typical Charpy V-Notch Properties
As Welded | |
Impact Value | 48 ft-lb |
Impact Value | 65 J |
Shielding Gas | ISO |
Testing Temperature | 68 °F |
Testing Temperature | 20 °C |
Typical Tensile Properties
Condition | Elongation | Shielding Gas | Tensile Strength | Yield Strength |
As Welded | 35 % | ISO | 590 MPa (86 ksi) | 410 MPa (59 ksi) |
Deposition Data
Current | Deposition Rate @ 90% I max | Diameter | Deposition Efficiency (%) | Number of electrodes/kg weld metal | Voltage | |
60-85 A | 44 sec | 0.9 kg/h (2.0 lb/h) | 2.5 x 300.0 mm (0.098 x 11.8 in.) | 60 % | 91 | 24 V |
85-130 A | 60 sec | 1.5 kg/h (3.3 lb/h) | 3.2 x 350.0 mm (1/8 x 13.8 in.) | 58 % | 41 | 27 V |
95-180 A | 64 sec | 1.9 kg/h (4.2 lb/h) | 4.0 x 350.0 mm (5/32 x 13.8 in.) | 51 % | 30 | 29 V |
Classifications
Classifications |
EN ISO 3581-A : E 20 25 5 Cu N L R 3 2 SFA/AWS A5.4 : E385-16 Werkstoffnummer : 1.4519 |
Approvals
Approvals |
CE EN 13479 VdTÜV 02805 |
Approvals are based on factory location. Please contact ESAB for more information. |
Consumable Characteristics
Alloy Type | Austenitic CrNiMo |
Coating Type | Basic Rutile |
Ferrite Content | FN 0 |
Welding Current | AC, DC+ |
Typical Weld Metal Analysis %
Typical Weld Metal Analysis % | ||||||||||||||
C | Cr | Cu | Mn | Mo | Ni | Si | ||||||||
0.03 % | 20 % | 1.5 % | 1 % | 4.7 % | 25 % | 0.5 % |